فارسی | English

In order to view this object you need Flash Player 9+ support!

Get Adobe Flash player

About Products

Portland Cement Type II

Analysis:


Faraz Firouzkouh Cement Certificate


Quality Certificate
Cement Specification: Type II

Chemical Composition:

Std Elements min - max Factores min - max Std
  Silicon Dioxiod Sio2 21.0 22.5 Insoluble Residue I.R 0.2 0.5 0.75 (max)
  Aluminium Oxide Al203 4.7 5.5 Free Lime F.CaO 0.4 1  
  Ferric Oxide Fe2O3 3.8 4.2 Lime Saturation Factor LSF 92 94  
  Calcium Oxide CaO 63 65 Silica Module SiM 2.35 2.45  
%5 (max) Magnesium Oxide MgO 1.5 2.2 Alumina Module AM 1.15 1.35  
%3 (max) Sulphur Oxide SO3 1.5 2.5 Tricalcium Silicate C3S 50 60  
  Potassium Oxide K2O 0.45 0.65 Dicalcium Silicate C2S 15 25  
  Sodium Oxide Na2O 0.45 0.65 Tricalcium Aluminate C3A 5.5 7.5 8% (max)
  Loss On lgnition LOI 1.0 2.0 Tricalcium Alumino Ferrit C4AF 10 12  

Physical Tests:

      min max Standard
Fineness Blain Test (cm2/gr) >2900 2800 (min)
Autoclave Expansion   (%) 0.05 0.15 0.8 (max)
Setting Time:          
  Initial (Minute) 100 160 45 (min)
  Final (Minute) 180 240 360 (max)
Compressive Strengt:          
  3 days kg/cm2 150 250 100 (min)
  7 days kg/cm2 250 350 175 (min)
  28 days kg/cm2 400 500 325 (min)


Clinker Specification

Chemical Composition:

Std Elements min max Factors min max Std
  Silicon Dioxiod Sio2 21.5 22.5 Lime Saturation Factors LSF 91 94  
  Aluminium Oxide Al2O3 4.5 5 Free Lime F.CaO 0.5 1.5  
  Ferric Oxide Fe2O3 4 4.5 Litre Weight L.W 1150 1350  
  Calcium Oxide CaO 63 65        
  Magnesium Oxide MgO 0.5 1        
  Sulphur Oxide SO3 0.5 1        
  Potassium Oxide K2O 0.4 0.7        
  Sodium Oxide Na2O 0.2 0.5        
  Loss On lgnition LOI 0.5 1        


Loading and delivery:

Bulk: Bulk in Mini Bunker and Bunker
Bag: In 50Kg Polypropylene (P.P) Bags

Production Process

The raw materials include alluvium as the main material, limestone and iron ore as additives.

All about cement

The raw materials include alluvium as the main material, limestone and iron ore as additives. Also, Gypsum (4%) is used as additive to cement.